MIM technology has a shape change itself,
but such change is predictable and usually is isotropic.And only commonly occur
during sintering, so-called deformation is in the shape of irregular change,
green of the binder concentration gradient in capillary force sufficient to
cause warp, crack, and our goal is to minimize size deviation, and dimensional
deviation depends on the size of the process in the process of control, this is
one of the problems of MIM technology early, sintering conditions, conditions
of geometric shapes and metal injection molding small changes will lead to big
dimension deviation, sintering process due to the formation of sintering neck
between powder particles, green strength.