Skim the carbon content is a common problem
in the control, skim the existence of residual carbon is likely to cemented
carbide and silicon carbide, steel and other materials is good, but for other
materials such as stainless steel, aluminum oxide is extremely harmful,
magnetic materials, control of carbon is an important aspect in defatted
practice, for some lack of stable carbide material system control carbon is a
particular problem, carbon content is through the control of degreasing
atmosphere and the choice of heating rate, if the temperature reached 450
degrees about polymer binder still not removal, so residual binder can cause
carbon residue problems, to get a lower carbon content, note the following: the
thermal degreasing late heating rate must be low, under the low temperature
heat preservation, high gas dew point and the atmosphere of high flow rate.
Original article link:http://www.zcmim.com/article/a-common-problem-of_1.html