In
order to facilitate forming, MIM technology has added a large number of binder
(15~20%) in its raw materials. These binders must be removed completely before
sintering process. Different feedstock system requires different ways of degreasing. As majority of
enterprises are not familiar with the use of feedstock, they can not use
debinding technology correctly and reasonably. Any debinding defect will affect
sintered products quality directly and affect products yield rate directly. Equipment
failure is mostly caused by improper operation in process of debinding, which
is not related to the structure and quality of equipment.