MIM green fracture strength of 3-20 mpa,
green strength can be adjusted by powder and binder, usually, it is different
size and shape of powder mixed together to increase the friction between the
particles, deformation usually occur in the early heating, because
thermoplastic binder softening and the intensity of lose, most prone to
deformation in about 150 c heat preservation.