MIM
process(http://www.zcmim.com/helps/mimprocess.html) requires three steps:
(1)
In condition of heating, pressure, injection the mixture of powdered metal and
thermoplastics (or other binder) into mold cavity (similar to thermoplastic
injection molding).
(2)
Removing binder by heating or melting, only the metal powder left.
(3)
Sintering the metal powder. Sintering temperature should be lower than the
melting point of metal, but enough to make metal powder combined into solid
metal (actual solid metal density is more than 96%).
Original article link:http://www.zcmim.com/article/mim-tmpot_1.html