Delamination in metal powder injection molding, process
is: finish
product present micaceous structure. It can be easily split between
layers
Analysis causes and find treatment for it:
- mix in dissimilar material
- temperature of material is too low
Analysis causes and find treatment for it:
- mix in dissimilar material
- temperature of material is too low
Cloudy phenomenon in metal powder injection molding process is: a layer of milky film coved product surface,
just like covered by mist, which make
insufficient glossiness. causes and treatment:
- rough mould and insufficient brightness
- mould and material’s temperature are too low
- rough mould and insufficient brightness
- mould and material’s temperature are too low
-improper use of mold release agent
- addition agent pyrolyse or gasify on mould surface
- addition agent pyrolyse or gasify on mould surface
Original
article link:http://www.zcmim.com/article/metalpowderinjectionmoldingprocess_1.html